It consists of a test chamber, a runner, a sample holder and a control panel. When conducting the test, the rubber sample is placed on the stand, and the test conditions such as load and speed are set on the control panel. The specimen holder is then rotated against the grinding wheel for a specified period of time. At the end of the test, the degree of wear is calculated by measuring the weight loss of the specimen or the depth of the wear track. Test results obtained from the Rubber Abrasion Resistance Akron Abrasion Tester are used to determine the abrasion resistance of rubber articles such as tires, conveyor belts, and shoe soles.
Applicable industries: rubber industry, shoe industry.
Determination of standard: GB/T1689-1998vulcanized rubber wear resistance machine(Akron)
ltem | Method A | Method B |
Test temperature | 75±2"C | 75+2°℃ |
Speed of spindle | 1200+60 r/min | 1200+60 r/min |
Testing time | 60±1min | 60±1min |
Axial testing force | 147N(15kgf) | 392N(40kgf) |
Axial testing force zero point inductance | ±1.96N(±0.2kgf) | ±1.96N(o.2kgf) |
Standard steel-ball specimen | 12.7mm | 12.7mm |
Name | rubber wear resistance akron abrasion testing machine |
Grinding wheel size | Diameter of 150mm, the thickness of 25m, center hole diameter of 32mm; particle size of 36,abrasive alumina |
Sand wheel | D150mm,W25mm, particle size 36 # combine |
Specimen size Note: D for rubber tire diameter, h is the thickness of the sample |
Strip [length (D+2 h)of+0~5mm,12.7±0.2mm; thickness of 3.2mm,±0.2mm] Rubber Wheel diameter 68 °-1mm, thickness of 12.7±0.2mm, hardness of 75 to 80 degrees |
Specimen tilt angle range | " to 35 ° adjustable |
Weight weight | Each of 2lb,6Lb |
Transfer speed | BS250±5r/min;GB76±2r/min |
Counter | 6-digit |
Motor specifications | 1/4HP[O.18KW) |
Size of the machine | 65cmx50cmx40cm |
The weight of the machine | 6Okg |
Balance hammer | 2.5Kg |
Counter | |
Power Supply | single phase AC 220V 3A |